Asphalt Mix Types

Every mix designation used in Pakistan, with density, typical layer, thickness and the standard it is specified under.

Project dimensions

Full cost breakdown
Use this often? Press Ctrl+D (or ⌘+D on Mac) to bookmark this calculator so it's one tap away next time.

Mix types

DesignationDescriptionDensity (kg/m³)Typical useStandard
Asphaltic Concrete Wearing CourseClass A / Class B2,34040–50 mm wearing courseNHA GS Item 305
Asphaltic Base CourseABC2,36050–100 mm baseNHA GS Item 306
Asphalt Treated BaseATB2,350Heavy-duty baseNHA GS
Bituminous MacadamOpen-graded base2,180Profile correctionNHA GS
Triple Surface TreatmentTST / chip sealSurface dressingNHA GS Item 303
SMAStone Matrix Asphalt2,400Heavy traffic corridorsAASHTO M 325
Recycled asphalt (RAP)Milled material2,000Base, shoulders, access tracksAASHTO M 323
Aggregate Base CourseGranular base2,200150–300 mmNHA GS Item 304
Sub-baseGranular sub-base2,150150–300 mmNHA GS
Bitumen 60/70Penetration grade binder1,030Binder and tack coatAASHTO M 20
Bitumen 80/100Penetration grade, cold regions1,025Northern areasAASHTO M 20
Emulsion, tack coatCationic emulsion1,010Between liftsNHA GS Item 302
Asphalt density by mix typeHorizontal bar chart of compacted asphalt density by mix type, ranging from porous asphalt at 100 pounds per cubic foot to EME 2 at 152 pounds per cubic foot, with dense-graded hot mix asphalt at 145.Compacted asphalt density by mix typePorous / Permeable Asphalt100 lb/ft³ · 1,602 kg/m³Open-Graded Friction Course115 lb/ft³ · 1,842 kg/m³RAP Millings125 lb/ft³ · 2,002 kg/m³Bituminous Macadam135 lb/ft³ · 2,162 kg/m³Cold Mix Asphalt140 lb/ft³ · 2,243 kg/m³Warm Mix Asphalt143 lb/ft³ · 2,291 kg/m³Dense-graded HMA145 lb/ft³ · 2,323 kg/m³Bituminous Concrete147 lb/ft³ · 2,355 kg/m³Dense Bituminous Macadam148 lb/ft³ · 2,371 kg/m³BBSG 0/10148 lb/ft³ · 2,371 kg/m³Grave Bitume149 lb/ft³ · 2,387 kg/m³Stone Matrix Asphalt150 lb/ft³ · 2,403 kg/m³BBME150 lb/ft³ · 2,403 kg/m³EME 2152 lb/ft³ · 2,435 kg/m³AsphaltCalculatorPrice.com — values are nominal compacted in-place densities.
Compacted asphalt density by mix type, from porous asphalt at 100 lb/ft³ to EME 2 at 152 lb/ft³.

2026 prices

ItemLowTypicalHigh
Asphaltic Concrete Wearing Course per ton₨25,000₨27,500₨32,000
Asphaltic Base Course per ton₨22,500₨25,000₨29,000
Bituminous Macadam per ton₨19,500₨22,000₨26,000
SMA per ton₨32,000₨36,000₨42,000
RAP / recycled per ton₨3,000₨5,500₨9,000
Aggregate Base Course per ton₨3,200₨4,200₨5,600
Bitumen 60/70 per ton₨185,000₨210,000₨235,000
Bitumen 80/100 per ton₨188,000₨214,000₨240,000
Road surfacing per m² (AC 50 mm)₨1,450₨1,850₨2,400
Full flexible pavement per m²₨4,200₨5,800₨8,200

Recommended thickness

ApplicationSurface courseBinder / base courseUnbound base
Village access roadTST surface dressing150 mm ABC
Residential street40 mm AC wearing50 mm ABC200 mm aggregate base
Urban road50 mm AC wearing75 mm ABC250 mm aggregate base
Provincial highway50 mm AC wearing100 mm ABC250 mm base + 200 mm sub-base
National highway50 mm AC wearing125–175 mm ABC300 mm base + 250 mm sub-base
Motorway50 mm SMA or AC175–225 mm ABC300 mm base + 300 mm sub-base
Industrial yard50 mm AC100 mm ABC300 mm base
Parking area40 mm AC50 mm ABC200 mm base

Waste and compaction allowance

Loose material behind the paver occupies roughly 20% more volume than the finished compacted surface. Add edge trimming, material left in the vehicle body and normal measurement tolerance, and you need an allowance on top of the calculated tonnage.

SituationAllowanceReason
Simple rectangle, machine-laid, experienced crew5%Minimal trimming and predictable compaction
Standard driveway or car park10%Normal edge detail and some hand work at the perimeter
Curved edges or several separate zones15%More offcuts and more hand placement
Hand-laid work and small patches15%Hand compaction is less consistent
Recycled planings15–20%Higher compaction factor and less predictable spread
Unbound granular base20–25%Significant consolidation under the roller

Round the final figure up to the nearest half tonne. Being short means a cold joint in the middle of the surface and a second delivery charge, which costs far more than the extra material would have.

The base underneath

The unbound layer under the surfacing does more structural work than the surfacing itself, and it is where most premature failures actually originate. A thinner bound layer over a deep, well-compacted, free-draining base will outlast a thicker bound layer over a shallow one.

SubgradeApproximate CBRBase under domestic accessBase under commercial
Well-graded gravel20–40100 mm150 mm
Sand, well drained10–20100–150 mm150–200 mm
Silty sand6–10150 mm200 mm
Loam5–8150–200 mm200–250 mm
Silty clay3–5200–250 mm250–300 mm
Heavy clay, poorly drained2–3250–300 mm plus geotextile300–450 mm plus stabilisation
Peat or organic soilunder 2Excavate and replaceExcavate and replace

Two additions repay their cost on marginal ground: a separation geotextile between the subgrade and the granular layer, which stops stone punching down into soft clay and can save 50–100 mm of aggregate; and proof-rolling with a loaded vehicle before any stone is placed, which finds the soft spots while they are still cheap to deal with.

Remember that the granular base is usually the larger tonnage of the two. A 100 m² area with 200 mm of base at 2,100 kg/m³ needs 42 tonnes of stone against roughly 12 tonnes of surfacing at 50 mm. Budget and order for both.

Standards and who administers them

Surfacing work in Pakistan is specified under NHA General Specifications and AASHTO material standards, administered by the National Highway Authority (NHA) and provincial highway departments. In practice that governs three things you will see on any quotation or drawing:

For private domestic work none of this is legally binding, but the same physics applies. Asking a contractor which specification they are working to, and getting the compacted thickness written into the quotation in millimetres, is the single most useful thing you can do to make competing quotations comparable.

Diagnosing surface problems

What you seeWhere it originatesWhat to do
Loose aggregate on the surface (ravelling)Wearing course — oxidised binderSurface dressing or a thin overlay
Longitudinal depressions in the wheel path (rutting)Wearing or binder coursePlane off and replace with a stiffer mix
Interconnected polygonal crackingStructural — base or subgradeReconstruction; an overlay will reflect through within two years
Straight cracks along the paving lineConstruction jointSeal, then overlay
Regular cracks across the carriagewayBinder grade against climateSeal; specify a softer low-temperature binder next time
Localised low spots and pondingSubgrade settlementExcavate, rebuild the formation and repave that area
Crumbling edgesUnsupported edgeBackfill against the edge or install an edge restraint
PotholesWater plus existing crackingFull-depth patch, then fix the drainage that caused it

Maintenance schedule

IntervalActionWhy it matters
Within the first 48 hoursKeep all vehicles offThe mat is still cooling and takes a permanent impression easily.
First 30 daysAvoid turning the wheel while stationary; support trailer jacks on a boardThe binder has not fully hardened and point loads leave marks.
Within 6–12 monthsFirst surface dressing or seal, if specifiedSlows oxidation of the binder. Applying it sooner traps volatiles and softens the surface.
AnnuallySweep, clear drainage, inspect edges and jointsStanding water at an edge is the most common cause of premature failure.
Every 1–2 yearsSeal any cracks that have appearedA sealed crack costs a fraction of the pothole it becomes.
Every 3–5 yearsReseal and, on car parks, re-lineRestores surface texture and appearance.
Every 10–15 yearsConsider a surface course overlayResets the wearing layer while the structure below survives.
20–25 yearsFull reconstructionOnly when the structure itself has failed, not merely the surface.

Deferred maintenance compounds quickly. A crack sealed early costs very little; the same crack left for two winters admits water, softens the base and becomes a full-depth patch. The economics of surfacing maintenance are almost entirely about intervening before water reaches the layers below.

Calculator

Frequently asked questions

How many tonnes do I need?

Area in m² × compacted thickness in m × 2.34. A 100 m² area at 50 mm needs about 11.7 tonnes.

How many m² does a tonne cover?

About 8.5 m² at 50 mm compacted.

What allowance should I add?

10% for standard work, 5% for simple machine-laid rectangles, 15% for curved or hand-laid areas.

Does the calculator handle several areas?

Yes — add a zone per shape, each with its own thickness and mix type. Multi-layer structures and irregular sites are entered directly.

Which standards apply?

NHA General Specifications and AASHTO material standards, administered by the National Highway Authority (NHA) and provincial highway departments.

Sources and further reading

Last reviewed: Next review: November 2026 Reviewed by: AsphaltCalculatorPrice Editorial TeamRegion: Pakistan