Bitumen Mix Types

Every mix designation used in India, with density, typical layer, thickness and the standard it is specified under.

Project dimensions

Full cost breakdown
Use this often? Press Ctrl+D (or ⌘+D on Mac) to bookmark this calculator so it's one tap away next time.

Mix types

DesignationDescriptionDensity (kg/m³)Typical useStandard
BC — Bituminous ConcreteWearing course2,35530–50 mm wearing courseMoRTH Clause 509
SDBC — Semi-Dense Bituminous ConcreteThin wearing course2,33025–30 mmMoRTH Clause 508
DBM — Dense Bituminous MacadamBinder / base course2,37050–100 mmMoRTH Clause 507
BM — Bituminous MacadamOpen-graded base2,16050–75 mm profile courseMoRTH Clause 504
Premix carpetThin open-graded surfacing2,00020 mm rural surfacingMoRTH Clause 511
Mix seal surfacingThin surfacing with seal2,05020 mmMoRTH Clause 512
SMAStone Matrix Asphalt2,400High-traffic wearing courseIRC SP:79
BC with modified binderPMB wearing course2,365Heavy traffic corridorsIRC SP:53
RAP / recycled mixReclaimed bituminous material2,000Base and shouldersIRC 120
WMM — Wet Mix MacadamGranular base2,200150–250 mm baseMoRTH Clause 406
GSB — Granular Sub-BaseUnbound sub-base2,150150–300 mmMoRTH Clause 401
VG-30 bitumenViscosity grade binder1,030Binder and tack coat onlyIS 73
Asphalt density by mix typeHorizontal bar chart of compacted asphalt density by mix type, ranging from porous asphalt at 100 pounds per cubic foot to EME 2 at 152 pounds per cubic foot, with dense-graded hot mix asphalt at 145.Compacted asphalt density by mix typePorous / Permeable Asphalt100 lb/ft³ · 1,602 kg/m³Open-Graded Friction Course115 lb/ft³ · 1,842 kg/m³RAP Millings125 lb/ft³ · 2,002 kg/m³Bituminous Macadam135 lb/ft³ · 2,162 kg/m³Cold Mix Asphalt140 lb/ft³ · 2,243 kg/m³Warm Mix Asphalt143 lb/ft³ · 2,291 kg/m³Dense-graded HMA145 lb/ft³ · 2,323 kg/m³Bituminous Concrete147 lb/ft³ · 2,355 kg/m³Dense Bituminous Macadam148 lb/ft³ · 2,371 kg/m³BBSG 0/10148 lb/ft³ · 2,371 kg/m³Grave Bitume149 lb/ft³ · 2,387 kg/m³Stone Matrix Asphalt150 lb/ft³ · 2,403 kg/m³BBME150 lb/ft³ · 2,403 kg/m³EME 2152 lb/ft³ · 2,435 kg/m³AsphaltCalculatorPrice.com — values are nominal compacted in-place densities.
Compacted asphalt density by mix type, from porous asphalt at 100 lb/ft³ to EME 2 at 152 lb/ft³.

2026 prices

ItemLowTypicalHigh
Bituminous Concrete (BC) per MT₹6,200₹6,800₹7,900
DBM per MT₹5,600₹6,200₹7,200
BM per MT₹4,900₹5,500₹6,400
Premix carpet per MT₹4,600₹5,200₹6,100
SMA per MT₹7,600₹8,500₹9,800
RAP / recycled per MT₹700₹1,400₹2,400
WMM per MT₹950₹1,250₹1,650
VG-30 bitumen per MT₹48,000₹52,000₹58,000
Road surfacing per m² (BC 40 mm)₹320₹420₹560
Full flexible pavement per m²₹1,100₹1,650₹2,400

Recommended thickness

ApplicationSurface courseBinder / base courseUnbound base
Village / rural road20 mm premix carpet75 mm WBM/BM150 mm GSB
Residential colony road25 mm SDBC50 mm DBM150 mm WMM + 150 mm GSB
Urban local road30–40 mm BC50–75 mm DBM250 mm WMM + 200 mm GSB
State highway40 mm BC75–100 mm DBM250 mm WMM + 200 mm GSB
National highway40–50 mm BC100–150 mm DBM250 mm WMM + 200–300 mm GSB
Expressway50 mm SMA or BC (PMB)150–190 mm DBM250 mm WMM + 300 mm GSB
Industrial yard40 mm BC100 mm DBM300 mm WMM
Parking area30 mm BC50 mm DBM200 mm WMM

Waste and compaction allowance

Loose material behind the paver occupies roughly 20% more volume than the finished compacted surface. Add edge trimming, material left in the vehicle body and normal measurement tolerance, and you need an allowance on top of the calculated tonnage.

SituationAllowanceReason
Simple rectangle, machine-laid, experienced crew5%Minimal trimming and predictable compaction
Standard driveway or car park10%Normal edge detail and some hand work at the perimeter
Curved edges or several separate zones15%More offcuts and more hand placement
Hand-laid work and small patches15%Hand compaction is less consistent
Recycled planings15–20%Higher compaction factor and less predictable spread
Unbound granular base20–25%Significant consolidation under the roller

Round the final figure up to the nearest half tonne. Being short means a cold joint in the middle of the surface and a second delivery charge, which costs far more than the extra material would have.

The base underneath

The unbound layer under the surfacing does more structural work than the surfacing itself, and it is where most premature failures actually originate. A thinner bound layer over a deep, well-compacted, free-draining base will outlast a thicker bound layer over a shallow one.

SubgradeApproximate CBRBase under domestic accessBase under commercial
Well-graded gravel20–40100 mm150 mm
Sand, well drained10–20100–150 mm150–200 mm
Silty sand6–10150 mm200 mm
Loam5–8150–200 mm200–250 mm
Silty clay3–5200–250 mm250–300 mm
Heavy clay, poorly drained2–3250–300 mm plus geotextile300–450 mm plus stabilisation
Peat or organic soilunder 2Excavate and replaceExcavate and replace

Two additions repay their cost on marginal ground: a separation geotextile between the subgrade and the granular layer, which stops stone punching down into soft clay and can save 50–100 mm of aggregate; and proof-rolling with a loaded vehicle before any stone is placed, which finds the soft spots while they are still cheap to deal with.

Remember that the granular base is usually the larger tonnage of the two. A 100 m² area with 200 mm of base at 2,100 kg/m³ needs 42 tonnes of stone against roughly 12 tonnes of surfacing at 50 mm. Budget and order for both.

Standards and who administers them

Surfacing work in India is specified under MoRTH Specifications for Road and Bridge Works and IRC codes, administered by MoRTH, NHAI and the Indian Roads Congress. In practice that governs three things you will see on any quotation or drawing:

For private domestic work none of this is legally binding, but the same physics applies. Asking a contractor which specification they are working to, and getting the compacted thickness written into the quotation in millimetres, is the single most useful thing you can do to make competing quotations comparable.

Diagnosing surface problems

What you seeWhere it originatesWhat to do
Loose aggregate on the surface (ravelling)Wearing course — oxidised binderSurface dressing or a thin overlay
Longitudinal depressions in the wheel path (rutting)Wearing or binder coursePlane off and replace with a stiffer mix
Interconnected polygonal crackingStructural — base or subgradeReconstruction; an overlay will reflect through within two years
Straight cracks along the paving lineConstruction jointSeal, then overlay
Regular cracks across the carriagewayBinder grade against climateSeal; specify a softer low-temperature binder next time
Localised low spots and pondingSubgrade settlementExcavate, rebuild the formation and repave that area
Crumbling edgesUnsupported edgeBackfill against the edge or install an edge restraint
PotholesWater plus existing crackingFull-depth patch, then fix the drainage that caused it

Maintenance schedule

IntervalActionWhy it matters
Within the first 48 hoursKeep all vehicles offThe mat is still cooling and takes a permanent impression easily.
First 30 daysAvoid turning the wheel while stationary; support trailer jacks on a boardThe binder has not fully hardened and point loads leave marks.
Within 6–12 monthsFirst surface dressing or seal, if specifiedSlows oxidation of the binder. Applying it sooner traps volatiles and softens the surface.
AnnuallySweep, clear drainage, inspect edges and jointsStanding water at an edge is the most common cause of premature failure.
Every 1–2 yearsSeal any cracks that have appearedA sealed crack costs a fraction of the pothole it becomes.
Every 3–5 yearsReseal and, on car parks, re-lineRestores surface texture and appearance.
Every 10–15 yearsConsider a surface course overlayResets the wearing layer while the structure below survives.
20–25 yearsFull reconstructionOnly when the structure itself has failed, not merely the surface.

Deferred maintenance compounds quickly. A crack sealed early costs very little; the same crack left for two winters admits water, softens the base and becomes a full-depth patch. The economics of surfacing maintenance are almost entirely about intervening before water reaches the layers below.

Calculator

Frequently asked questions

How many tonnes do I need?

Area in m² × compacted thickness in m × 2.35. A 100 m² area at 50 mm needs about 11.8 tonnes.

How many m² does a tonne cover?

About 8.5 m² at 50 mm compacted.

What allowance should I add?

10% for standard work, 5% for simple machine-laid rectangles, 15% for curved or hand-laid areas.

Does the calculator handle several areas?

Yes — add a zone per shape, each with its own thickness and mix type. Multi-layer structures and irregular sites are entered directly.

Which standards apply?

MoRTH Specifications for Road and Bridge Works and IRC codes, administered by MoRTH, NHAI and the Indian Roads Congress.

Sources and further reading

Last reviewed: Next review: November 2026 Reviewed by: AsphaltCalculatorPrice Editorial TeamRegion: India